+ | New bottle of Deuterated Silane (SiD4) has been installed, we are running process qualifications. |
||
⚫ | |||
+ | |||
⚫ | |||
+ | We don't yet have a tracking number for the Hardware delivery, so it's possible it does not arrive tomorrow (due to supply chain problems). We are expecting to have ASML engineers on-site next week to begin some of the repairs. Tool will be down into next week at least, depending on the hardware delivery schedule. We have possibly repaired two of the failures that required new hardware - will verify next week when ASML engineers are on-site. |
||
⚫ | |||
===== Masks Optional as of June 13 ===== |
===== Masks Optional as of June 13 ===== |
||
Line 26: | Line 34: | ||
The temperature controller on the PureStrip vertical bath in Bay 4 acid bench has failed, do not attempt to use until we replace it. |
The temperature controller on the PureStrip vertical bath in Bay 4 acid bench has failed, do not attempt to use until we replace it. |
||
// [[User:John d|John d]] 16:09, 10 June 2022 (PDT) |
// [[User:John d|John d]] 16:09, 10 June 2022 (PDT) |
||
− | |||
⚫ | |||
− | Hardware delivery ETA updated to June 17th. |
||
− | We’ll schedule an ASML engineer on-site visit to perform the installation, verification and system calibrations. |
||
− | We may have been able to revive the TCU, but have another electrical hardware failure that requires a new part from ASML. |
||
⚫ | |||
===== Gasonics Down ===== |
===== Gasonics Down ===== |
||
Leak in main chamber, tool is down. |
Leak in main chamber, tool is down. |
||
// [[User:John d|John d]] 14:35, 27 May 2022 (PDT) |
// [[User:John d|John d]] 14:35, 27 May 2022 (PDT) |
||
− | |||
⚫ | |||
− | Deuterated Silane (SiD4) is out. Bottle expected to be delivered on Monday 6/13. |
||
⚫ | |||
===== New EBL Rates ===== |
===== New EBL Rates ===== |
Revision as of 10:26, 16 June 2022
Important Announcements
Unaxis-Dep: Qualifying
New bottle of Deuterated Silane (SiD4) has been installed, we are running process qualifications. // John d 10:26, 16 June 2022 (PDT)
ASML Down
We don't yet have a tracking number for the Hardware delivery, so it's possible it does not arrive tomorrow (due to supply chain problems). We are expecting to have ASML engineers on-site next week to begin some of the repairs. Tool will be down into next week at least, depending on the hardware delivery schedule. We have possibly repaired two of the failures that required new hardware - will verify next week when ASML engineers are on-site. // John d 10:26, 16 June 2022 (PDT)
Masks Optional as of June 13
You are not required to wear a mask in UC buildings at this time. You are also not required to wear a mask in the Nanofab if desired.
We will still provide masks at the metal table in front of the cleanroom entry. See the UCSB announcement at this link.
See the full policies at COVID-19_User_Policies // John d 11:20, 13 June 2022 (PDT)
PureStrip Bath Heater DOWN
The temperature controller on the PureStrip vertical bath in Bay 4 acid bench has failed, do not attempt to use until we replace it. // John d 16:09, 10 June 2022 (PDT)
Gasonics Down
Leak in main chamber, tool is down. // John d 14:35, 27 May 2022 (PDT)
New EBL Rates
Effective Dec.1, 2021, all of our electron beam lithography rates are lowered. The new rates are as follows:
Industrial Users: $405/hour
UC Academic Users: $126/hour
Non-UC Academic Users: $150/hour
UCSB CNSI Incubator USers: $260/hour
//Thibeault 12:21, 9 December 2021 (PST)