===== New Filmetrics Systems =====
  +
We are in the process of installing a Filmetric F10-RT, for obtaining optical transmission & reflection measurements and measuring thin-film properties such as thickess, refractive index and absorption. We are also installing a thin-film wafer-mapping system, the Filmetrics F50. Trainings will be announced one operating procedures have been developed.
 
// [[User:John d|John d]] 08:08, 9 November 2018 (PST)
   
 
===== RIE#5: Software Upgrades =====
 
===== RIE#5: Software Upgrades =====
Line 17: Line 21:
 
Software upgrade completed, everyone must be re-certified to use the tool. All old recipe files have been backed up but not reinstated - let us know if you need your old recipe parameters.
 
Software upgrade completed, everyone must be re-certified to use the tool. All old recipe files have been backed up but not reinstated - let us know if you need your old recipe parameters.
 
// [[User:John d|John d]] 14:39, 16 October 2018 (PDT)
 
// [[User:John d|John d]] 14:39, 16 October 2018 (PDT)
 
===== CARY500 - Down - Decomissioned =====
 
CARY 500 Spectrophotometer has failed - Will not be repaired - being decomissioned. New Filmetrics F10-RT-UVX being ordered as a replacement.
 
// [[User:Thibeault|Thibeault]] 16:40, 26 September 2018 (PDT)
 
   
 
<!---------- end of announcements ------------>
 
<!---------- end of announcements ------------>

Revision as of 09:08, 9 November 2018

UCSB NanoFab Announcements

New Filmetrics Systems

We are in the process of installing a Filmetric F10-RT, for obtaining optical transmission & reflection measurements and measuring thin-film properties such as thickess, refractive index and absorption. We are also installing a thin-film wafer-mapping system, the Filmetrics F50. Trainings will be announced one operating procedures have been developed. // John d 08:08, 9 November 2018 (PST)

RIE#5: Software Upgrades

RIE#5 system has undergone a software upgrade. All users will need to be retrained to use the new Cortex software. // John d 14:39, 16 October 2018 (PDT)

PECVD#1: Software Upgrade