Line 20: | Line 20: | ||
The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. See the [[ASML 5500 Mask Making Guidelines|Mask Making Guidelines page]] for more info on exposure field sizes and how to order your mask plates. |
The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. See the [[ASML 5500 Mask Making Guidelines|Mask Making Guidelines page]] for more info on exposure field sizes and how to order your mask plates. |
||
− | Resists Used (see [https://www.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes PhotoLith. Recipes] for |
+ | Resists Used (see [https://www.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes PhotoLith. Recipes] for full process info): |
* UV210-0.3 - Positive: 300nm nominal thickness |
* UV210-0.3 - Positive: 300nm nominal thickness |
||
* UV6-0.8 - Positive: 800nm nominal thickness |
* UV6-0.8 - Positive: 800nm nominal thickness |
||
Line 37: | Line 37: | ||
*Minimum Feature Size: ≤150 nm isolated lines, ≤200 nm dense patterns |
*Minimum Feature Size: ≤150 nm isolated lines, ≤200 nm dense patterns |
||
*Maximum Wafer Bow: approx. 100 µm. (4-inch diam.). |
*Maximum Wafer Bow: approx. 100 µm. (4-inch diam.). |
||
− | **'' |
+ | **''Near this value, and the job may fail or lose the wafer inside the machine due to wafer vacuum error.'' |
+ | *[[ASML Stepper 3 - UCSB Test Reticles|UCSB Test Reticles - Alignment Markers, Resolution Testing etc.]] |
||
=Service Provider= |
=Service Provider= |
||
Line 47: | Line 48: | ||
* [[media:ASML Job Set-Up Guide simple v1.pdf|Job Programming- Simplified -Full Wafers]] |
* [[media:ASML Job Set-Up Guide simple v1.pdf|Job Programming- Simplified -Full Wafers]] |
||
* [[ASML 5500 Mask Making Guidelines|ASML 5500 Mask Making Guidelines]] |
* [[ASML 5500 Mask Making Guidelines|ASML 5500 Mask Making Guidelines]] |
||
− | * [[ASML Stepper 3 - UCSB Test Reticles|UCSB Test Reticles - Alignment Markers etc.]] |
||
=== Troubleshooting and Recovery === |
=== Troubleshooting and Recovery === |
||
Line 60: | Line 60: | ||
* [[ASML 5500: Choose Marks for Prealignment]] |
* [[ASML 5500: Choose Marks for Prealignment]] |
||
− | ** ''If your job aborted with "Alignment failure" on the E- or P-Chuck, because it |
+ | ** ''If your job aborted with "Alignment failure" on the E- or P-Chuck, because it your alignment marks are damaged, this is how to edit your job to use different alignment marks.'' |
Revision as of 13:25, 28 August 2018
|
Contents
About
The ASML 5500 stepper is a 248nm DUV stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. Overlay accuracy is better than 30nm.
The system is configured for 4” wafers and, with staff support, mounted pieces down to 14mm in size can be exposed using a 4” wafer as a carrier. The system is designed for high throughput, so shooting multiple 4" wafers is extremely fast. Additionally, exposure jobs are highly programmable, allowing for very flexible exposures of multiple aligned patterns from multiple masks in a single session, allowing for process optimization of large vs. small features in a single lithography.
The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. See the Mask Making Guidelines page for more info on exposure field sizes and how to order your mask plates.
Resists Used (see PhotoLith. Recipes for full process info):
- UV210-0.3 - Positive: 300nm nominal thickness
- UV6-0.8 - Positive: 800nm nominal thickness
- UV26-2.5 - Positive: 2.5um nominal thickness
- UVN2300-0.5 - Negative: 500nm nominal thickness
- AR2/DUV42P-6/DS-K101: Anti-Reflective Coatings
- PMGI: Underlayer
AZ300MIF Developer for all processes
Process Information
- Process Page
- Alignment Accuracy: < 50 nm
- Minimum Feature Size: ≤150 nm isolated lines, ≤200 nm dense patterns
- Maximum Wafer Bow: approx. 100 µm. (4-inch diam.).
- Near this value, and the job may fail or lose the wafer inside the machine due to wafer vacuum error.
- UCSB Test Reticles - Alignment Markers, Resolution Testing etc.
Service Provider
Operating Procedures
- Standard Operating Procedure
- Job Programming - Full
- Job Programming- Simplified -Full Wafers
- ASML 5500 Mask Making Guidelines
Troubleshooting and Recovery
- Error Recovery, Troubleshooting and Calibration
- Common errors, Wafer Retrieval, General error recovery, and system calibration check
- ASML 5500: Recovering from an Error
- How to abort the job and recover your wafer.
- ASML 5500: Recovering from a Typo in Reticle ID
- If you ran a job and got "Reticle Not Present" due to a typo in your job/layer/image's reticle ID.
- ASML 5500: Choose Marks for Prealignment