Line 17: | Line 17: | ||
==Ta{{sub|2}}O{{sub|5}} deposition (IBD)== |
==Ta{{sub|2}}O{{sub|5}} deposition (IBD)== |
||
*{{fl|IBD-Ta2O5-Recipe.pdf|Ta{{sub|2}}O{{sub|5}} dep}} |
*{{fl|IBD-Ta2O5-Recipe.pdf|Ta{{sub|2}}O{{sub|5}} dep}} |
||
+ | |||
+ | ==TiO{{sub|2}} deposition (IBD)== |
||
+ | *{{fl|IBD-TiO2-Recipe.pdf|TiO{{sub|2}} dep}} |