Revision as of 13:17, 28 June 2012 by Zwarburg (talk | contribs) (Created page with " Max temp/Time 1000C = 1 Hour 1100C = 10 min 1200C = 3 min 1300C = 10 seconds")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search


Max temp/Time

1000C = 1 Hour 1100C = 10 min 1200C = 3 min 1300C = 10 seconds