==CdZnTe Etching (RIE 2)==
 
==CdZnTe Etching (RIE 2)==
 
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]]
 
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]]
  +
  +
==InP-InGaAsP-InGaAlAs Etching (RIE 2)==
  +
*[[media:RIE2-InGaAs-InP-InAlAs-Etch-Plasma-RIE-RevA.pdf|InP-InGaAsP-InAlGaAs Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]]
   
 