Difference between revisions of "PECVD Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 36: Line 36:
 
=== SiN (2% SiH<sub>4</sub> - No-Ar) ===
 
=== SiN (2% SiH<sub>4</sub> - No-Ar) ===
 
*50°
 
*50°
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-5W-50C-High-Stress.pdf|SiN Deposition Recipe - No Ar (5W 50° High Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-50W-50C-Medium-Stress.pdf|SiN Deposition Recipe - No Ar (50W 50° Medium Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-120W-50C-Low-Stress.pdf|SiN Deposition Recipe - No Ar (120W 50° Low Stress)]]
**
 
 
*100°C
 
*100°C
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-5W-100C-High-Stress.pdf|SiN Deposition Recipe - No Ar (5W 100° High Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-50W-100C-Medium-Stress.pdf|SiN Deposition Recipe - No Ar (50W 100° Medium Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-120W-100C-Low-Stress.pdf|SiN Deposition Recipe - No Ar (120W 100° Low Stress)]]
**
 
 
*250°C
 
*250°C
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-5W-250C-High-Stress.pdf|SiN Deposition Recipe - No Ar (5W 250° High Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-50W-250C-Medium-Stress.pdf|SiN Deposition Recipe - No Ar (50W 250° Medium Stress)]]
**
 
  +
**[[Media:PECVD2-SiN-Recipe-NoAr-120W-250C-Low-Stress.pdf|SiN Deposition Recipe - No Ar (120W 250° Low Stress)]]
**
 

Revision as of 09:31, 20 August 2012

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

SiN (2% SiH4 - No-Ar)