Difference between revisions of "PECVD Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 68: Line 68:
 
*[https://docs.google.com/spreadsheets/d/1VI-sUmaqois0NsCvf2kQmPfRRa03MjBzl779hmmLtP4/edit#gid=sharing Oxide Data 2018]
 
*[https://docs.google.com/spreadsheets/d/1VI-sUmaqois0NsCvf2kQmPfRRa03MjBzl779hmmLtP4/edit#gid=sharing Oxide Data 2018]
 
*[https://docs.google.com/spreadsheets/d/1VI-sUmaqois0NsCvf2kQmPfRRa03MjBzl779hmmLtP4/edit#gid=sharing Oxide Data 2019]
 
*[https://docs.google.com/spreadsheets/d/1VI-sUmaqois0NsCvf2kQmPfRRa03MjBzl779hmmLtP4/edit#gid=sharing Oxide Data 2019]
 
 
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDRjSHEtYUZRUTg4azE2U0JGUTg2M1E#gid=sharing Oxide Thickness Uniformity 2014]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDRjSHEtYUZRUTg4azE2U0JGUTg2M1E#gid=sharing Oxide Thickness Uniformity 2014]
 
*[https://docs.google.com/spreadsheets/d/16pZHcGwesXB1mMPwntOudBIlPvRh6A6DI37DEwyYfPw/edit#gid=sharing Oxide Thickness Uniformity 2015]
 
*[https://docs.google.com/spreadsheets/d/16pZHcGwesXB1mMPwntOudBIlPvRh6A6DI37DEwyYfPw/edit#gid=sharing Oxide Thickness Uniformity 2015]
Line 76: Line 74:
 
*[https://docs.google.com/spreadsheets/d/1064j6894X63WlRX3Uolxg1q1FRzUZLqSZQA9BWwzPOk/edit#gid=sharing Oxide Thickness Uniformity 2018]
 
*[https://docs.google.com/spreadsheets/d/1064j6894X63WlRX3Uolxg1q1FRzUZLqSZQA9BWwzPOk/edit#gid=sharing Oxide Thickness Uniformity 2018]
 
*[https://docs.google.com/spreadsheets/d/1064j6894X63WlRX3Uolxg1q1FRzUZLqSZQA9BWwzPOk/edit#gid=sharing Oxide Thickness Uniformity 2019]
 
*[https://docs.google.com/spreadsheets/d/1064j6894X63WlRX3Uolxg1q1FRzUZLqSZQA9BWwzPOk/edit#gid=sharing Oxide Thickness Uniformity 2019]
  +
   
 
*[[media:New Adv PECVD OXIDE 300C standard recipe OXIDE Standard Recipe.pdf|Oxide Standard Recipe 2014-5/9/18]]
 
*[[media:New Adv PECVD OXIDE 300C standard recipe OXIDE Standard Recipe.pdf|Oxide Standard Recipe 2014-5/9/18]]

Revision as of 15:53, 2 January 2019

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

Note: Software upgrade performed on 2018-10-10. Note any changes in film.


SiN deposition (PECVD #1)


SiO2 deposition (PECVD #1)


OTHER recipes: Low-Stress (LS) SiN and SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiO2 deposition (PECVD #2)


SiN deposition (PECVD #2)



Low-Stress SiN deposition (PECVD #2)

Low-Stress SilIcon Nitride (< 100 MPa)


Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° (pinholes) 100° (pinholes) 250°

SiN (100% SiH4 )

50° (pinholes) 100° (pinholes) 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°