*[[Media:PECVD2-SiN-Recipe-Medium stress SiNx-100%SiH4-120W-50C.pdf|SiN Deposition Recipe (120W 50° Medium Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-Medium stress SiNx-100%SiH4-120W-50C.pdf|SiN Deposition Recipe (50W 50° Medium Stress)]]
 
|
 
|
*[[Media:PECVD2-SiN-Recipe-Medium stres SiNx-100% SiH4-120W-100C.pdf|SiN Deposition Recipe (120W 100° Medium Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-Medium stres SiNx-100% SiH4-120W-100C.pdf|SiN Deposition Recipe (50W 100° Medium Stress)]]
*[[Media:PECVD2-SiN-Table-Low stres SiNx-100% SiH4-120W-100C.pdf|SiN Comparison Table 120W, 100(250)C]]
+
*[[Media:PECVD2-SiN-Table-Low stres SiNx-100% SiH4-120W-100C.pdf|SiN Comparison Table 50W, 100(250)C]]
 
*[[Media:PECVD2-SiN-SEM- Medium stres SiNx-100% SiH4-120W-100C.pdf|SiN SEM sidewall coverage]]
 
*[[Media:PECVD2-SiN-SEM- Medium stres SiNx-100% SiH4-120W-100C.pdf|SiN SEM sidewall coverage]]
 
|
 
|
*[[Media:PECVD2-SiN-Recipe-Medium stress SiNx-100% SiH4-120W-250C.pdf|SiN Deposition Recipe (120W 250° Medium Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-Medium stress SiNx-100% SiH4-120W-250C.pdf|SiN Deposition Recipe (50W 250° Medium Stress)]]
*[[Media:PECVD2-SiN-Table-Low stres SiNx-100% SiH4-120W-100C.pdf|SiN ComparisonTable 120W, 100(250)C]]
+
*[[Media:PECVD2-SiN-Table-Low stres SiNx-100% SiH4-120W-100C.pdf|SiN ComparisonTable 50W, 100(250)C]]
 
|-
 
|-
 
|}
 
|}

Revision as of 14:04, 5 October 2012

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

50° 100° 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°