==SiN deposition (Unaxis VLR) ==
 
==SiN deposition (Unaxis VLR) ==
 
=== SiN (2% SiH<sub>4</sub>) ===
 
=== SiN (2% SiH<sub>4</sub>) ===
  +
{| border="1" class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"
*50°
 
  +
|- bgcolor="#D0E7FF"
**[[Media:PECVD2-SiN-Recipe-5W-50C-High-Stress.pdf|SiN Deposition Recipe (5W 50° High Stress)]]
 
  +
!width=350 align=center|50°
**[[Media:PECVD2-SiN-Recipe-50W-50C-Medium-Stress.pdf|SiN Deposition Recipe (50W 50° Medium Stress)]]
 
  +
!width=350 align=center|100°
**[[Media:PECVD2-SiN-Recipe-120W-50C-Low-Stress.pdf|SiN Deposition Recipe (120W 50° Low Stress)]]
 
  +
!width=350 align=center|250°
*100°C
 
  +
|-align=left
**[[Media:PECVD2-SiN-Recipe-5W-100C-High-Stress.pdf|SiN Deposition Recipe (5W 100° High Stress)]]
 
  +
|
**[[Media:PECVD2-SiN-Recipe-50W-100C-Medium-Stress.pdf|SiN Deposition Recipe (50W 100° Medium Stress)]]
 
**[[Media:PECVD2-SiN-Recipe-120W-100C-Low-Stress.pdf|SiN Deposition Recipe (120W 100° Low Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-5W-50C-High-Stress.pdf|SiN Deposition Recipe (5W 50° High Stress)]]
 
*[[Media:PECVD2-SiN-Recipe-50W-50C-Medium-Stress.pdf|SiN Deposition Recipe (50W 50° Medium Stress)]]
*250°C
 
**[[Media:PECVD2-SiN-Recipe-5W-250C-High-Stress.pdf|SiN Deposition Recipe (5W 250° High Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-120W-50C-Low-Stress.pdf|SiN Deposition Recipe (120W 50° Low Stress)]]
  +
|
**[[Media:PECVD2-SiN-Recipe-50W-250C-Medium-Stress.pdf|SiN Deposition Recipe (50W 250° Medium Stress)]]
 
**[[Media:PECVD2-SiN-Recipe-120W-250C-Low-Stress.pdf|SiN Deposition Recipe (120W 250° Low Stress)]]
+
*[[Media:PECVD2-SiN-Recipe-5W-100C-High-Stress.pdf|SiN Deposition Recipe (5W 100° High Stress)]]
 
*[[Media:PECVD2-SiN-Recipe-50W-100C-Medium-Stress.pdf|SiN Deposition Recipe (50W 100° Medium Stress)]]
 
*[[Media:PECVD2-SiN-Recipe-120W-100C-Low-Stress.pdf|SiN Deposition Recipe (120W 100° Low Stress)]]
  +
|
 
*[[Media:PECVD2-SiN-Recipe-5W-250C-High-Stress.pdf|SiN Deposition Recipe (5W 250° High Stress)]]
 
*[[Media:PECVD2-SiN-Recipe-50W-250C-Medium-Stress.pdf|SiN Deposition Recipe (50W 250° Medium Stress)]]
 
*[[Media:PECVD2-SiN-Recipe-120W-250C-Low-Stress.pdf|SiN Deposition Recipe (120W 250° Low Stress)]]
  +
|-
  +
|}
   
 
=== SiN (2% SiH<sub>4</sub> - No-Ar) ===
 
=== SiN (2% SiH<sub>4</sub> - No-Ar) ===

Revision as of 09:41, 20 August 2012

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

SiN (2% SiH4 - No-Ar - Extra N2)