PECVD 2 (Advanced Vacuum)
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
|
About
- Films/Gases: This open-load system is dedicated to PECVD of SiO2, SiNx, SiOxNy, and a-Si using Silane (2%SiH4, 98% He), N2O, NH3, and N2 gases.
- Size: The sample electrode has a 270mm diameter useable area, allowing for multiple 4” wafer depositions in a single run.
- Temperature: Standard operating temperature is 300C, but can be user changed for temps ranging anywhere from 250 to 350C.
- Low-Stress Si3N4: The system is equipped with a dual generator, dual frequency option for growth of Low-stress Nitride films.
- The Low-Stress Si3N4 film recipe are tested approx. monthly, and kept within ±100MPa. Data can be found at Recipes (below) > Low-Stress Nitride.
See Also
Documentation
- Operating Instructions
- Wafer Coating Process Traveler
- For particle counting method, see the Surfscan Scanning Procedure
Recipes & Historical Data
- Recipes can be found on the PECVD Recipes Page:
- Recipes > Vacuum Deposition Recipes > PECVD Recipes > PECVD 2 - Advanced Vacuum
- Thin-Films recorded: SiO2, Si3N4 and Low-Stress Si3N4
- Historical (Process Control) Data is also shown here.
- A list of all available deposited films can be found on the Vacuum Deposition Recipes page: