Difference between revisions of "PECVD 2 (Advanced Vacuum)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(moved recipes to bottom (like other pages))
Line 2: Line 2:
 
|picture=PECVD2.jpg
 
|picture=PECVD2.jpg
 
|type = Vacuum Deposition
 
|type = Vacuum Deposition
|super= Brian Lingg
+
|super= Don Freeborn
|phone=(805)839-3918x219
+
|phone=(805)839-7975
 
|location=Bay 2
 
|location=Bay 2
 
|email=silva@ece.ucsb.edu
 
|email=silva@ece.ucsb.edu
 
|description = Vision 310 Advanced Vacuum PECVD
 
|description = Vision 310 Advanced Vacuum PECVD
|manufacturer = Veeco
+
|manufacturer = Plasma-Therm
 
|materials =  
 
|materials =  
 
|toolid=15
 
|toolid=15

Revision as of 20:06, 27 October 2021

PECVD 2 (Advanced Vacuum)
PECVD2.jpg
Tool Type Vacuum Deposition
Location Bay 2
Supervisor Don Freeborn
Supervisor Phone (805) 893-7975
Supervisor E-Mail dfreeborn@ece.ucsb.edu
Description Vision 310 Advanced Vacuum PECVD
Manufacturer Plasma-Therm
Vacuum Deposition Recipes
Sign up for this tool


About

This open-load system is dedicated to PECVD of SiO2, SiNx, SiOxNy, and a-Si using Silane (2%SiH4, 98% He), N2O, NH3, and N2 gases. The sample electrode has a 270mm diameter useable area, allowing for multiple 4” wafer depositions in a single run. Standard operating temperature is 300C, but can be user changed for temps ranging anywhere from 250 to 350C. The system is equipped with a dual generator, dual frequency option for growth of low-stress Nitride films.

See Also

Documentation

Recipes & Historical Data