Tool Type Thermal Processing
Location various
Description Lab ovens
Manufacturer various
Thermal Processing Recipes


See the full list of Thermal Processing tools here.

List of all lab ovens and capabilities/uses
Oven Name + Link Temperature Range/Capabilities Programmable Gases Vacuum/Pressure Range Typical Uses SignupMonkey Reservation
Oven 1
  • Typically 95°C
  • Passive Cooling
No, single temperature. N/A Atmosphere only Drying glassware, general baking. No. Users may change temperature.
Oven 2
  • Typically 100°C
  • Passive Cooling
No, single temperature. N/A Atmosphere only Drying glassware, general baking. No. Users may change temperature.
Oven 4: HeraTherm Oven
  • Multi-step programmable
  • Ramp Rate: only low/med/high (not numeric ramp rate).
  • Gas flow not programmable
  • N2 (manual flow setting)
  • Atmosphere Purge
Atmosphere only Bonding, BCB/Polymer curing. No

Reserve with note in logbook.

Blue-M Oven
  • Max. temp. 350°C
  • Passive Cooling
  • Yes, fully programmable up to 2 stages.
  • Gas flow not programmable
  • N2 (manual flow setting)
Atmosphere only BCB/Polymer curing. Sign Up For This Tool
YES Vacuum Oven