Revision as of 10:21, 30 August 2022

About

The oven temperature can be controlled from 30C-200C with a user programable ramp rate between 0.1C-1.0C/min. Maximum temperature is 200C. There is a N2 purge to provide a dry intert atmosphere during use.

Documentation

Oven 5

Oven 5 (Labline)
Oven5.jpg
Location Bay 5
Tool Type Lithography
Manufacturer Labline
Description ?


Secondary Supervisor

Aidan Hopkins


Recipes N/A