Difference between revisions of "Oven 4 (Thermo-Fisher HeraTherm)"
Jump to navigation
Jump to search
(added info, needs verification) |
|||
(5 intermediate revisions by 3 users not shown) | |||
Line 1: | Line 1: | ||
− | {{ |
+ | {{tool2|{{PAGENAME}} |
|picture=Oven4.jpg |
|picture=Oven4.jpg |
||
|type = Lithography |
|type = Lithography |
||
− | |super= |
+ | |super= Michael Barreraz |
+ | |super2= Aidan Hopkins |
||
|location=Bay 6 |
|location=Bay 6 |
||
|description = Programmable Oven |
|description = Programmable Oven |
||
|manufacturer = Thermo Scientific |
|manufacturer = Thermo Scientific |
||
|model = HeraTherm |
|model = HeraTherm |
||
+ | |toolid=68 |
||
}} |
}} |
||
− | == |
+ | ==About== |
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven. |
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven. |
||
− | == |
+ | ==Specifications== |
⚫ | |||
⚫ | |||
⚫ | |||
⚫ | |||
⚫ | |||
⚫ | |||
⚫ | |||
− | * {{todo|User Manual}} |
||
⚫ | |||
⚫ | |||
+ | |||
⚫ | |||
+ | |||
+ | * |
||
+ | {{Instructions}} |
||
+ | |||
+ | [https://wiki.nanotech.ucsb.edu/w/images/8/8e/Heratherm_instructions.pdf Instructions] |
||
+ | |||
+ | <br /> |
Latest revision as of 16:25, 13 September 2022
|
About
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven.
Specifications
- Maximum Temperature = 330 C (no active cooling)
- Gases: N2, manually set with needle valve (not programmable)
- Multi-step programmable temperature ramps
- Programmable atmospheric purge (for cooling)