Difference between revisions of "Other Dry Etching Recipes"
Jump to navigation
Jump to search
Line 2: | Line 2: | ||
=[[XeF2 Etch (Xetch)]]= |
=[[XeF2 Etch (Xetch)]]= |
||
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] |
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] |
||
+ | |||
+ | =[[Vapor HF Etch (uETCH)]]= |
||
+ | *[[media:|Si Etch Recipe]] |