Difference between revisions of "Molecular Vapor Deposition"
(added recipe link) (Tag: Visual edit) |
(Text replacement - "www.nanotech.ucsb.edu/wiki/" to "wiki.nanotech.ucsb.edu/wiki/") |
||
Line 15: | Line 15: | ||
==Recipes== |
==Recipes== |
||
− | *[https:// |
+ | *[https://wiki.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Nanoimprinting_Recipes Nanoimprinting recipes] using FDTS non-stick layer |
*[https://signupmonkey.ece.ucsb.edu/wiki/images/3/3c/MVD_Standard_Recipes.pdf MVD Standard Recipes] |
*[https://signupmonkey.ece.ucsb.edu/wiki/images/3/3c/MVD_Standard_Recipes.pdf MVD Standard Recipes] |
||
Revision as of 18:26, 6 April 2020
|
About
The Molecular Vapor deposition system is used for deposition of a monolayer-thick fluorocarbon film for producing extremely hydrophobic surfaces used for anti-sticking layers for nanoimprinting or anti-stiction layers for MEMS. The system has integrated Oxygen plasma cleaning for organic removal and surface activation and can be run at temperatures up to 80°C. Multi-step recipes can be created. The system is currently configured for FDTS (perflourodecyltricholorsilane) and water to producing the coatings. Up to 6” wafers can be coated in the system.
Recipes
- Nanoimprinting recipes using FDTS non-stick layer
- MVD Standard Recipes