Mechanical Polisher (Allied)
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
|
About
The Allied Polisher allows for bulk thinning of substrates, and fine polishing of optical waveguide facets. Various materials are typically lapped/polished, such as Silicon GaAs, InP.
Detailed Specs
- Max. Substrate Size
- Lapping Films available:
- 10µm AlOx
- 5µm AlOx
- 2µm AlOx
- 1µm AlOx
- 0.5 AlOx
Operating Procedures
Recipes
- To Be Added