Difference between revisions of "Direct-Write Lithography Recipes"
Jump to navigation
Jump to search
m (→Greyscale Lithography: added model to header title) |
|||
Line 17: | Line 17: | ||
! width="75" |Thickness |
! width="75" |Thickness |
||
!Laser (nm) |
!Laser (nm) |
||
− | ! width="125" |Exposure Time |
+ | ! width="125" |Exposure Time| |
! width="100" |DeFocus |
! width="100" |DeFocus |
||
! width="75" |PEB |
! width="75" |PEB |
||
Line 29: | Line 29: | ||
|~ 1.1 µm |
|~ 1.1 µm |
||
|405 |
|405 |
||
− | | |
+ | |240 |
− | | |
+ | |5 |
|''none'' |
|''none'' |
||
|AZ400K:DI 1:4 |
|AZ400K:DI 1:4 |
||
|50s |
|50s |
||
+ | |Used MLA design (good for isolated lines 0.8-1um) |
||
− | | |
||
|- |
|- |
||
|[[:File:AXP4000pb-Datasheet.pdf|AZ4330]] |
|[[:File:AXP4000pb-Datasheet.pdf|AZ4330]] |
||
Line 96: | Line 96: | ||
| |
| |
||
|} |
|} |
||
+ | |||
=== Negative Resist (MLA150) === |
=== Negative Resist (MLA150) === |
||
''General notes: Hotplates used, filters, laser wavelengths, etc.'' |
''General notes: Hotplates used, filters, laser wavelengths, etc.'' |
Revision as of 11:38, 9 October 2020
Work In Progress This article is still under construction. It may contain factual errors. Content is subject to change. |
Maskless Aligner (Heidelberg MLA150)
Photolithography Recipes for the Heidelberg MLA150. Description of litho params- different lasers available, greyscale etc.
Positive Resist (MLA150)
General notes: Hotplates used, filters, laser wavelengths, etc.
Resist | Spin Cond. | Bake | Thickness | Laser (nm) | Exposure Time| | DeFocus | PEB | Developer | Developer Time | Comments |
---|---|---|---|---|---|---|---|---|---|---|
AZ4110 | 4 krpm/30s | 95°C/60s | ~ 1.1 µm | 405 | 240 | 5 | none | AZ400K:DI 1:4 | 50s | Used MLA design (good for isolated lines 0.8-1um) |
AZ4330 | 4 krpm/30s | 95°C/60s | ~ 3.3 µm | 405 | none | AZ400K:DI 1:4 | 90s | |||
AZ4620 | ||||||||||
SPR 220-3.0 | 2.5 krpm/30s | 115°C/90” | ~ 2.7 µm | 405 | 115°C/90s | AZ300MIF | 60s | |||
SPR 955-CM0.9 | 3 krpm/30s | 95°C/60” | ~ 0.9 µm | 405 | 110°C/60s | AZ300MIF | 60s | |||
THMR-3600HP |
Negative Resist (MLA150)
General notes: Hotplates used, filters, laser wavelengths, etc.
Resist | Spin Cond. | Bake | Thickness | Laser (nm) | Exposure Time | DeFocus | PEB | Flood | Developer | Developer Time | Comments |
---|---|---|---|---|---|---|---|---|---|---|---|
AZ5214 | 6 krpm/30s | 95°C/60s | ~ 1.0 µm | 405 | 60" | AZ300MIF | 60s |
| |||
AZnLOF2020 | 3 krpm/30s | 110°C/90s | ~ 2.1µm | 405 | none | AZ300MIF | 60s | ||||
SU-8 2075 | ~70µm | 375 | Extremely viscous. Pour into a wide-mouthed bottle, dispense directly from bottle. Replace napkin at end. |
Greyscale Lithography (MLA150)
Description...
Resist | Spin Cond. | Bake | Thickness | Exposure Time | Focus Offset | PEB | Flood | Developer | Developer Time | Comments |
---|---|---|---|---|---|---|---|---|---|---|
AZ4620Z5214 | ?? krpm/30” | 95°C/60” | ?? µm | 60" | AZ300MIF | 60" |
|