Logitech WBS7 - Procedure for Wax Mounting with Spin-On Crystalbond
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
Work In Progress This article is still under construction. It may contain factual errors. Content is subject to change. |
Draft only - in progress. Based on Don Freeborn's procedure for the Logitech Bonder. -- Demis 2018-10-16
- Mix a fresh squirt bottle of CrystalBond diluted with Acetone (see Don Freeborn for method).
- XYZ grams of crystalbond, mixed into
- XYZ mL of Acetone, in dedicated squirt bottle
- Shake/stir to completely dissolve the wax
- Place 4-inch silicon carrier wafer on POLOS spinner in solvent bench, with non-vacuum 4-inch chuck installed.
- Set up POLOS recipe
- Spin at XYZ rpm for XYZ sec.
- Squirt wax solution onto wafer
- I/O to spin.
- Place carrier wafer on Logitech bonder surface
- Place sample to be bonded on top
- Place 110mm chemical filter paper on top
- Close lid, secure lid clamp
- Run recipe:
- XYZ °C
- XYZ seconds
- Vacuum etc.?