Lift-Off Techniques
Description/Tutorial
Bi-Layer Process with PMGI Underlayer and Contact Aligner
Lithography Recipes
Contact Aligners
Steppers
Flood Expose
E-Beam Lithography
Positive Resists
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ4110
R
AZ4210
R
AZ4330RS
R
OCG 825-35CS
SPR 950-0.8
SPR 955 CM-0.9
SPR 955 CM-1.8
SPR 220-3.0
R
SPR 220-7.0
R
THMR-IP3600 HP D
UV6-0.7
Negative Resists
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ5214-EIR
R
AZnLOF 2020
R
AZnLOF 2035
AZnLOF 2070
AZnLOF P5510
UVN30-0.5
SU-8 2015
Underlayers
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
PMGI SF-11
PMGI SF-15
LOL 2000
XHRIC-11 (BARC)
AR-2 (BARC)
DS-K 101-307 (BARC)
Overlayers
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
CEM-365 IS
E-Beam Resists
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
??????
???????
Nanoimprint Resists
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
MR-I 7020
Nanonex NX-1020
SUSS MJB-3
SUSS MA-6
Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
Variants
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
COVID-19 Protocols
Common Questions
Staff List
Equipment Signup
Chemicals + MSDS
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Inspection, Test & Characterization
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Calculators/Utilities
Facility Data
Usage
Research
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information