Difference between revisions of "Lithography Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 16: Line 16:
 
*{{fl|AZnLOF2020-Negative-Resist-Datasheet.pdf|AZnLOF2020}}
 
*{{fl|AZnLOF2020-Negative-Resist-Datasheet.pdf|AZnLOF2020}}
 
;Underlayers
 
;Underlayers
*{{fl|PMGI-Underlayer-Datasheet.pdf|PMGI (PMGI SF-11, PMGI SF-13, PMGI SF-15}}
+
*{{fl|PMGI-Underlayer-Datasheet.pdf|PMGI (PMGI SF-11, PMGI SF-13, PMGI SF-15)}}
 
*{{fl|LOL2000-Underlayer-Datasheet.pdf|Shipley LOL2000}}
 
*{{fl|LOL2000-Underlayer-Datasheet.pdf|Shipley LOL2000}}
  +
;E-beam resists
  +
*{{fl|PMMA-E-Beam-Resist-Datasheet.pdf|PMMA (PMMA, P(MMA-MAA) copolymer)}}
  +
*{{fl|maN2403-E-Beam-Resist-Datasheet.pdf|maN 2403}}
   
 
==Recipes==
 
==Recipes==

Revision as of 17:03, 8 November 2012

Lift-Off Techniques

Chemical Datasheets

To Do: Ask Brian where these should go...
Positive Photoresists
Negative Photoresists
Underlayers
E-beam resists

Recipes

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.
Lithography Recipes

Contact Aligners Steppers Flood Expose E-Beam Lithography
Positive Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ4110 R R
AZ4210 R R





AZ4330RS R R
OCG 825-35CS







SPR 950-0.8
SPR 955 CM-0.9







SPR 955 CM-1.8
SPR 220-3.0 R R





SPR 220-7.0 R R
THMR-IP3600 HP D







UV6-0.7
Negative Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ5214-EIR R R
AZnLOF 2020 R R
AZnLOF 2035
AZnLOF 2070
AZnLOF P5510
UVN30-0.5
SU-8 2015
Underlayers SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
PMGI SF-11







PMGI SF-15
LOL 2000
XHRIC-11 (BARC)
AR-2 (BARC)
DS-K 101-307 (BARC)
Overlayers SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
CEM-365 IS
E-Beam Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
??????
???????
Nanoimprint Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
MR-I 7020
Nanonex NX-1020
SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)