Difference between revisions of "KLayout Design Tips"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(pasted more tips from Calc+Utilities page)
(Added Editing Mode)
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
*The default minimum unit of 0.001 µm (1nm) is usually fine. Don't change this after drawing - everything will be scaled accordinglyIf you need finer resolution, ''Before'' starting your design, set the '''''Layout Properties > Database Unit''''' to something smaller, eg. 0.0001 µm.
+
__TOC__
 +
 
 +
=== Turn on Editing Mode ===
 +
By default, KLayout might open as a "viewer" only, without draw-mode capbilities (no square/polygon/text buttons in the toolbar) and only ruler/zoom toolsEnable Editing mode as so:
 +
 
 +
* '''''Preferences > Editing mode > [√] Use Editing Mode by default''''', and restart the software.
  
 
===Turn on the display of the Origin (0,0)===
 
===Turn on the display of the Origin (0,0)===
  
 
*'''''Preferences > Display > Background > Axis''''' = change from the default "invisible", eg. "'''''Lines with Ticks'''''".
 
*'''''Preferences > Display > Background > Axis''''' = change from the default "invisible", eg. "'''''Lines with Ticks'''''".
 +
 +
===Minimum Step-Size / Database Unit===
 +
 +
*The default minimum unit of 0.001 µm (1nm) is usually fine. Don't change this after drawing - all polygons will be scaled accordingly.  If you need finer resolution: ''Before'' starting your design, set the '''''Layout Properties > Database Unit''''' to something smaller, eg. 0.0001 µm.
  
 
===How to draw circles===
 
===How to draw circles===
  
*You have to draw a square, and then apply the function '''''Edit > Selection > Convert to PCell'' > Basic.CIRCLE'''. Sometimes these P-Cells don't convert properly at the photomask vendor, so make sure to run '''''Edit > Selection > Convert to Static Cell''''' (which converts to a polygon) before taping out to the vendor.
+
*You have to draw a square, and then apply the function '''''Edit > Selection > Convert to PCell'' > Basic.CIRCLE'''. Sometimes these P-Cells don't convert properly at the photomask vendor, so make sure to run '''''Edit > Selection > Convert to Static Cell''''' (which converts to a polygon) before sending to the vendor/machine.
 
**Another way is to convert a square to a polygon directly with '''''Edit>Selection>Round Corners''''' function with '''''Outer Corner Radius''''' = the desired circle radius (radius is not changeable afterards in this method, but computation may be faster for a large number of objects).
 
**Another way is to convert a square to a polygon directly with '''''Edit>Selection>Round Corners''''' function with '''''Outer Corner Radius''''' = the desired circle radius (radius is not changeable afterards in this method, but computation may be faster for a large number of objects).
 
**Klayout doesn't natively support circles because the GDS file format does not have a "circle" primitive built-in, so instead it creates a polygon. Make sure you include enough polygon points, eg. 32. See the [https://www.klayout.de/forum/discussion/142/making-circles forum help pages] on this for more info.
 
**Klayout doesn't natively support circles because the GDS file format does not have a "circle" primitive built-in, so instead it creates a polygon. Make sure you include enough polygon points, eg. 32. See the [https://www.klayout.de/forum/discussion/142/making-circles forum help pages] on this for more info.
  
=== Cells & Instances of Cells ===
+
===Cells & Instances of Cells===
It is highly recommended that you understand and use the concept of "Cells" in your design. This circumvents many problems with enormous file sizes (due to huge numbers of identical polygons), and if used properly, helps tremendously with programming the Stepper lithography machines. Links to documentation below:
+
It is highly recommended that you understand and use the concept of "Cells" in your design. This is critical for direct-write machines ([https://wiki.nanotech.ucsb.edu/wiki/E-Beam_Lithography_System_(JEOL_JBX-6300FS) EBL], [https://wiki.nanotech.ucsb.edu/wiki/Maskless_Aligner_(Heidelberg_MLA150) MLA], Mask-writing vendors), and if used properly, helps tremendously with programming the Stepper lithography machines. This functionality also circumvents many with enormous file sizes (due to huge numbers of identical polygons), by "pointing" to the same polygon only defined once in the file. Links to documentation below:
  
 
*Create a new cell, and instancing that cell: [https://www.klayout.de/doc-qt4/manual/create_instance.html KLayout Docs : Creating a Cell instance]
 
*Create a new cell, and instancing that cell: [https://www.klayout.de/doc-qt4/manual/create_instance.html KLayout Docs : Creating a Cell instance]
*Viewing only some levels of the heirachy, to prevent drawing all objects: [https://www.klayout.de/doc/manual/hier.html KLayout Docs: Viewing Cell Heirarchy]
+
*Viewing only some levels of the Cell heirarchy, to prevent drawing all objects: [https://www.klayout.de/doc/manual/hier.html KLayout Docs: Viewing Cell Heirarchy]
  
=== File Types ===
+
===File Types===
 
OASIS files tend to be much smaller than GDS files, and they also save the Layer Names (not just Layer Number). Most Photomask manufacturers accept this file type.
 
OASIS files tend to be much smaller than GDS files, and they also save the Layer Names (not just Layer Number). Most Photomask manufacturers accept this file type.
  
GDS files are considered "standard", but are somewhat antiquated.
+
GDS files are considered "standard", but are somewhat antiquated, and lose the text names of layers between saves.
  
 
Alternatively, in KLayout the function '''File > Save Session''' will save the entire view including layer styles and window/zoom locations will be saved. You can share this file, as the entire design file is embedded within it, but it may not be as robust between KLayout versions.
 
Alternatively, in KLayout the function '''File > Save Session''' will save the entire view including layer styles and window/zoom locations will be saved. You can share this file, as the entire design file is embedded within it, but it may not be as robust between KLayout versions.
  
DXF files coming from AutoCAD often are missing the "units", and may erroneously map millimeters to meters, causing your design to be 1000x too large.  You can fix this in '''''File > Reader Options > DXF''''', or simply instance the entire design into a new Cell with Magnification set to correct the scaling error.
+
DXF files coming from AutoCAD often are missing the "units", and may erroneously map millimeters to meters, causing your design to be 1000x too large.  You can fix this in '''''File > Reader Options > DXF''''', or simply instance the entire design into a new Cell with Magnification set to correct the scaling error.  Also, AutoCAD allows for non-closed polygons, which are invalid shapes (even though the start/end points lie on top of each other, the shape is not technically "closed" unless you use polyline-edit "''PEDIT''" and intentionally Close them).  The DXF Reader has some options to catch/fix these.
===Non-Orthogonal Arrays (Important)===
+
===Non-Orthogonal Arrays===
 
Arrays created with diagonal instancing (non-orthogonal arrays) can be incompatible with photomask vendor's mask writing software.
 
Arrays created with diagonal instancing (non-orthogonal arrays) can be incompatible with photomask vendor's mask writing software.
  
 
We recommend you avoid the grey X and Y fields shown below when creating arrays, as shown here:
 
We recommend you avoid the grey X and Y fields shown below when creating arrays, as shown here:
 
[[File:KLayout - Non-Orthogonal Arrays.png|alt=Klayou screenshot showing non-orthogonal array definition|none|thumb|485x485px]]
 
[[File:KLayout - Non-Orthogonal Arrays.png|alt=Klayou screenshot showing non-orthogonal array definition|none|thumb|485x485px]]
If you do need to use a non-orthogonal array, make sure to use '''''Selection > Resolve Arrays''''' before submitting your design to the manufacturer.
+
If you do need to use a non-orthogonal array, make sure to use '''''Selection > Resolve Arrays''''' before submitting your design to the manufacturer/machine.

Latest revision as of 14:59, 1 March 2022

Turn on Editing Mode

By default, KLayout might open as a "viewer" only, without draw-mode capbilities (no square/polygon/text buttons in the toolbar) and only ruler/zoom tools. Enable Editing mode as so:

  • Preferences > Editing mode > [√] Use Editing Mode by default, and restart the software.

Turn on the display of the Origin (0,0)

  • Preferences > Display > Background > Axis = change from the default "invisible", eg. "Lines with Ticks".

Minimum Step-Size / Database Unit

  • The default minimum unit of 0.001 µm (1nm) is usually fine. Don't change this after drawing - all polygons will be scaled accordingly. If you need finer resolution: Before starting your design, set the Layout Properties > Database Unit to something smaller, eg. 0.0001 µm.

How to draw circles

  • You have to draw a square, and then apply the function Edit > Selection > Convert to PCell > Basic.CIRCLE. Sometimes these P-Cells don't convert properly at the photomask vendor, so make sure to run Edit > Selection > Convert to Static Cell (which converts to a polygon) before sending to the vendor/machine.
    • Another way is to convert a square to a polygon directly with Edit>Selection>Round Corners function with Outer Corner Radius = the desired circle radius (radius is not changeable afterards in this method, but computation may be faster for a large number of objects).
    • Klayout doesn't natively support circles because the GDS file format does not have a "circle" primitive built-in, so instead it creates a polygon. Make sure you include enough polygon points, eg. 32. See the forum help pages on this for more info.

Cells & Instances of Cells

It is highly recommended that you understand and use the concept of "Cells" in your design. This is critical for direct-write machines (EBL, MLA, Mask-writing vendors), and if used properly, helps tremendously with programming the Stepper lithography machines. This functionality also circumvents many with enormous file sizes (due to huge numbers of identical polygons), by "pointing" to the same polygon only defined once in the file. Links to documentation below:

File Types

OASIS files tend to be much smaller than GDS files, and they also save the Layer Names (not just Layer Number). Most Photomask manufacturers accept this file type.

GDS files are considered "standard", but are somewhat antiquated, and lose the text names of layers between saves.

Alternatively, in KLayout the function File > Save Session will save the entire view including layer styles and window/zoom locations will be saved. You can share this file, as the entire design file is embedded within it, but it may not be as robust between KLayout versions.

DXF files coming from AutoCAD often are missing the "units", and may erroneously map millimeters to meters, causing your design to be 1000x too large. You can fix this in File > Reader Options > DXF, or simply instance the entire design into a new Cell with Magnification set to correct the scaling error. Also, AutoCAD allows for non-closed polygons, which are invalid shapes (even though the start/end points lie on top of each other, the shape is not technically "closed" unless you use polyline-edit "PEDIT" and intentionally Close them). The DXF Reader has some options to catch/fix these.

Non-Orthogonal Arrays

Arrays created with diagonal instancing (non-orthogonal arrays) can be incompatible with photomask vendor's mask writing software.

We recommend you avoid the grey X and Y fields shown below when creating arrays, as shown here:

Klayou screenshot showing non-orthogonal array definition

If you do need to use a non-orthogonal array, make sure to use Selection > Resolve Arrays before submitting your design to the manufacturer/machine.