Si Deep RIE (PlasmaTherm/Bosch Etch)

Single-step Si Etching (not Bosch Process!) (Si Deep RIE)

ICP Etch 1 (Panasonic E626I)

SiO2 Etching (Panasonic 1)

SiNx Etching (Panasonic 1)

  • [[media:Panasonic1-SiN-Etch-Plasma-CF4-O2-ICP-revA.pdf|SiNx Etch Rates and Variations - CF4]-O2]

Al Etch (Panasonic 1)

Cr Etch (Panasonic 1)

Ti Etch (Panasonic 1)

AlGaAs Etch (Panasonic 1)

GaN Etch (Panasonic 1)

ICP Etch 2 (Panasonic E640)

SiO2 Etching (Panasonic 2)

SiNx Etching (Panasonic 2)

Al Etch (Panasonic 2)

GaAs Etch (Panasonic 2)

ICP-Etch (Unaxis VLR)

GaAs Etch

AlGaAs Etch

InP Etch (Unaxis VLR)

InP Etch

InP Etch (H2 Ar)

GaN Etch (Unaxis VLR)