Difference between revisions of "ICP Etching Recipes"
Jump to navigation
Jump to search
Line 25: | Line 25: | ||
− | =[[ |
+ | =[[XeF2 Etch (Xetch))]]= |
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] |
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] |
Revision as of 15:51, 18 September 2013
Back to Dry Etching Recipes.
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
Cr Etch (Panasonic 1)
GaN Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
ICP-Etch (Unaxis VLR)
InP Etch (Unaxis VLR)
InP Etch
InP Etch (H2 Ar)