Difference between revisions of "ICP Etching Recipes"
Jump to navigation
Jump to search
Line 3: | Line 3: | ||
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
||
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
||
+ | ==Cr Etch (Panasonic 1)== |
||
*[[media:CrEtch(Panasonic1).pdf|Cr Etch Recipes]] |
*[[media:CrEtch(Panasonic1).pdf|Cr Etch Recipes]] |
||
Revision as of 13:55, 18 June 2013
Back to Dry Etching Recipes.