*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
 
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
  
=[[XeF<sub>2</sub>2 Etch (Xetch))]]=
+
=[[XeF<sub>2</sub> Etch (Xetch))]]=
 
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]
 
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]