Line 21: Line 21:
 
===InP Etch (H<sub>2</sub> Ar)===
 
===InP Etch (H<sub>2</sub> Ar)===
 
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
 
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
 
 
 
  
 
=[[XeF2 Etch (Xetch))]]=
 
=[[XeF2 Etch (Xetch))]]=
 
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]
 
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]