Difference between revisions of "ICP Etching Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 3: Line 3:
 
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)==
 
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)==
 
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]]
 
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]]
 +
==SiO<sub>2</sub> Pure CHF3 Etch Recipe Variations (Panasonic 1)==
 +
*[[media:==SiO<sub>2</sub> Vertical Etch (Panasonic 1)|SiO<sub>2</sub> Vertical Etch Recipe]]
  
 
==Cr Etch (Panasonic 1)==
 
==Cr Etch (Panasonic 1)==

Revision as of 10:19, 30 August 2013