= Detailed Specifications = | = Detailed Specifications = | ||
− | *1000W ICP source, 600W RF Sample Bias | + | *1000W ICP source, 600W RF Sample Bias Power Supply |
*50 - 350°C sample temperature | *50 - 350°C sample temperature | ||
*100% SiH<sub>4</sub>, Ar, N<sub>2</sub>, O<sub>2</sub> | *100% SiH<sub>4</sub>, Ar, N<sub>2</sub>, O<sub>2</sub> | ||
*Multiple 4” diameter wafer capable system | *Multiple 4” diameter wafer capable system | ||
*Pieces possible by mounting or placing on 4 ” wafer | *Pieces possible by mounting or placing on 4 ” wafer |
Revision as of 14:24, 14 March 2014
|
About
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and RT-350°C operation. This chamber has 100% SiH4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be done down to below 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.
Detailed Specifications
- 1000W ICP source, 600W RF Sample Bias Power Supply
- 50 - 350°C sample temperature
- 100% SiH4, Ar, N2, O2
- Multiple 4” diameter wafer capable system
- Pieces possible by mounting or placing on 4 ” wafer