|picture=BlueMOven.jpg |
|picture=BlueMOven.jpg |
||
|type = Lithography |
|type = Lithography |
||
− | |super= |
+ | |super= Brian Lingg |
|location=Bay 5 |
|location=Bay 5 |
||
|description = High Temperature Oven |
|description = High Temperature Oven |
||
|manufacturer = Blue M Electric |
|manufacturer = Blue M Electric |
||
⚫ | |||
− | |materials = |
||
⚫ | |||
⚫ | |||
⚫ | |||
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide. |
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide. |
Revision as of 10:19, 15 April 2020
|
The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.