Goniometer
Goniometer.jpg
Tool Type Inspection, Test and Characterization
Location Bay 2
Supervisor Lee Sawyer
Supervisor Phone (805) 893-2123
Supervisor E-Mail lee_sawyer@ucsb.edu
Description Water Contact Angle
Manufacturer Ramé-Hart Instrument Co.
Model A-100


About

The goniometer enables measurement of the contact angle of water to a surface. The water contact angle is a measurement of how hydrophobic/hydrophilic a surface is. Such measurements can be important for analyzing/improving adhesion of thin-films or surfaces intended for wafer-bonding.