Difference between revisions of "Focused Ion-Beam Lithography (Raith Velion)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(added toolid, removed WIP, Pt dep/writing)
 
(3 intermediate revisions by one other user not shown)
Line 1: Line 1:
{{WIP}}
 
 
{{tool|{{PAGENAME}}
 
{{tool|{{PAGENAME}}
 
|picture=RaithVelion.jpg
 
|picture=RaithVelion.jpg
Line 6: Line 5:
 
|location=Bay 1
 
|location=Bay 1
 
|description = Focused Ion Beam Lithography
 
|description = Focused Ion Beam Lithography
|manufacturer = Raith Gmbh
+
|manufacturer = Raith GmbH
 
|model = Velion
 
|model = Velion
 
|materials =  
 
|materials =  
|toolid=
+
|toolid=69
 
}}  
 
}}  
 
= About  =
 
= About  =
The Raith Velion ion beam tool was installed at UCSB in 2020 and signed off and avaiable for. use in early 2021.
 
  
This system uses the vector scan approach for electron beam deflection within a field, step and repeat for stage movement between fields, the combination of which allows the entire area of the sample to be exposed to the electron beam.
+
VELION is a novel FIB-SEM instrument dedicated to advanced nanofabrication, in which FIB is the true priority technique. An evolution of Raith’s ionLINE, the ion column at the vertical position features a unique design to meet the most demanding nanofabrication requirements. It is supported by a field emission SEM solution as well as a highest-precision laser interferometer-controlled sample stage.
 +
 
 +
With its FIB-prioritized nanofabrication setup, including SEM and a high-accuracy stage, VELION allows for versatile use in four different operation modes that offer
 +
 
 +
• direct and versatile FIB patterning for simplified, flexible, 3D, and automated processing
 +
 
 +
• highest-precision nanofabrication over extended areas and periods of time with both FIB and SEM
 +
 
 +
• SEM imaging for in-situ process control, inspection and sample preparation.
  
The machine can be run at 25, 50 and 100 kV. Note however that only the 100kV mode is used at UCSB.
+
The Raith Velion ion beam tool was installed at UCSB in 2020 and signed off and avaiable for. use in early 2021.
  
 
=Detailed Specifications=
 
=Detailed Specifications=
Line 33: Line 39:
 
Additional Capabilities:  
 
Additional Capabilities:  
 
* Automated height sensing to detect sample surface height variation for automated correction
 
* Automated height sensing to detect sample surface height variation for automated correction
* Pt Gas Iinjection System (GIS) deposition
+
* Pt Gas Injection System (GIS) localized deposition/writing
 
*
 
*
* Raith Nanosuite software incl. CAD (GDSII) navigation & patterning
+
* Raith Nanosuite software including CAD (GDSII) navigation & patterning
 
== Recipes ==
 
== Recipes ==
 
* Recipes > Lithography > '''[[Lithography Recipes#FIB Lithography Recipes .28Raith Velion.29|<u>FIB Lithography</u>]]'''
 
* Recipes > Lithography > '''[[Lithography Recipes#FIB Lithography Recipes .28Raith Velion.29|<u>FIB Lithography</u>]]'''
 
** ''Contains starting recipes etc.''
 
** ''Contains starting recipes etc.''

Latest revision as of 09:56, 15 March 2021

Focused Ion-Beam Lithography (Raith Velion)
RaithVelion.jpg
Tool Type Lithography
Location Bay 1
Supervisor Dan Read
Supervisor Phone (805) 893-3138
Supervisor E-Mail dread@ucsb.edu
Description Focused Ion Beam Lithography
Manufacturer Raith GmbH
Model Velion
Sign up for this tool


About

VELION is a novel FIB-SEM instrument dedicated to advanced nanofabrication, in which FIB is the true priority technique. An evolution of Raith’s ionLINE, the ion column at the vertical position features a unique design to meet the most demanding nanofabrication requirements. It is supported by a field emission SEM solution as well as a highest-precision laser interferometer-controlled sample stage.

With its FIB-prioritized nanofabrication setup, including SEM and a high-accuracy stage, VELION allows for versatile use in four different operation modes that offer

• direct and versatile FIB patterning for simplified, flexible, 3D, and automated processing

• highest-precision nanofabrication over extended areas and periods of time with both FIB and SEM

• SEM imaging for in-situ process control, inspection and sample preparation.

The Raith Velion ion beam tool was installed at UCSB in 2020 and signed off and avaiable for. use in early 2021.

Detailed Specifications

nanoFIB column:

  • Liquid Metal Alloy Ion Sources (LMAIS) providing ions for Gallium-free patterning (Au, Si)
  • High resolution patterning capabilities (minimum feature size < 15nm)
  • Fully corrected write fields (distortion, stigmation)
  • Long term current stability (days)

Laser Interferometer stage:

  • Mechanical movement at 1nm precision
  • Continuous stage modes for stitch free FIB patterning on full 4”wafer scale
  • Stitching and overlay accuracy:  < 50 nm ( mean+3 sigma)

FE SEM

  • Process control for rapid prototyping

Additional Capabilities:  

  • Automated height sensing to detect sample surface height variation for automated correction
  • Pt Gas Injection System (GIS) localized deposition/writing
  • Raith Nanosuite software including CAD (GDSII) navigation & patterning

Recipes