R
= Recipe is available. Clicking this link will take you to the recipe.
A
= Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching
ICP Etching
Oxygen Plasma Systems
Other Dry Etchers
Material
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm)
ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Ag
A
Al
A
R
R
A
Au
R
Cr
A
R
A
A
Cu
A
Ge
A
A
Mo
A
Ni
R
Pt
R
Ru
A
R
A
Si
R
R
R
A
Ta
A
Ti
R
A
A
Al
2
O
3
R
A
Al
2
O
3 (Sapphire)
R
A
A
AlGaAs
R
R
R
A
AlGaN
R
A
AlN
R
A
CdZnTe
R
A
GaAs
R
R
R
R
A
GaN
R
R
R
A
GaSb
A
R
A
HfO
2
A
InGaAlAs
R
R
A
InGaAsP
R
R
A
InP
R
A
A
R
R
ITO
R
A
Photoresist
& ARC
A
R
R
R
A
A
A
A
SiC
R
A
A
SiN
R
R
R
A
A
SiO
2
R
A
R
R
R
A
SiOxNy
A
A
A
Ta
2
O
5
A
A
TiN
A
TiO
2
A
W-TiW
R
A
A
ZnO
2
A
ZnS
R
A
ZnSe
R
A
ZrO
2
A
Material
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Category
:
Processing
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
Variants
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
COVID-19 Protocols
Common Questions
Staff List
Equipment Signup
Chemicals + MSDS
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Inspection, Test & Characterization
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Calculators/Utilities
Facility Data
Usage
Research
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information