Difference between revisions of "Dry Etching Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 192: Line 192:
 
! bgcolor="#D0E7FF" align="center" | ITo  
 
! bgcolor="#D0E7FF" align="center" | ITo  
 
|  
 
|  
|  
+
| {{rl|RIE Etching Recipes|ITO Etch (RIE 2)}}
 
|  
 
|  
 
|  
 
|  
Line 355: Line 355:
 
! bgcolor="#D0E7FF" align="center" | InGaAlAs  
 
! bgcolor="#D0E7FF" align="center" | InGaAlAs  
 
|  
 
|  
| {{rl|RIE Etching Recipes|InP Etch (MRC)}}
+
| {{rl|RIE Etching Recipes|InP Etch (RIE 2)}}
 
|  
 
|  
 
|  
 
|  
Line 370: Line 370:
 
! bgcolor="#D0E7FF" align="center" | InGaAsP  
 
! bgcolor="#D0E7FF" align="center" | InGaAsP  
 
|  
 
|  
| {{rl|RIE Etching Recipes|InP Etch (MRC)}}
+
| {{rl|RIE Etching Recipes|InP Etch (RIE 2)}}
 
|  
 
|  
 
|  
 
|  
Line 385: Line 385:
 
! bgcolor="#D0E7FF" align="center" | InP  
 
! bgcolor="#D0E7FF" align="center" | InP  
 
|  
 
|  
| {{rl|RIE Etching Recipes|InP Etch (MRC)}}
+
| {{rl|RIE Etching Recipes|InP Etch (RIE 2)}}
 
|  
 
|  
 
|  
 
|  

Revision as of 17:04, 23 October 2013

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching ICP Etching Oxygen Plasma Systems Other Dry Etchers
Material RIE 1
(Custom)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PlasmaTherm/Bosch Etch)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Al R R
Ti R A
Cr A R A
Ge
Ag
Ru
Mo
Ta
W-TiW R A
Al2O3
HfO2
ITo R
SiO2 R R
SiN R R
SiOxNy
Ta2O5
TiO2
TiN
ZnO2
ZrO2
GaAs R R R
AlGaAs R R R
InGaAlAs R R
InGaAsP R
InP R R
GaN R R R
AlGaN
AlN
GaN
AlGaN
AlN
GaSb
CdZnTe R
ZnSe
Si R R
SiC
Sapphire
Material RIE 1
(Custom)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PlasmaTherm/Bosch Etch)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)