Difference between revisions of "Dry Etching Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(link to Fluorine etcher Ru-masked SiO2 etch.)
Line 574: Line 574:
 
|
 
|
 
|
 
|
|[[ICP Etching Recipes#SiO2 Etching|R]]
+
|{{rl|ICP Etching Recipes|SiO2 Etching (Fluorine ICP Etcher)}}
 
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 1)}}
 
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 1)}}
 
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 2)}}
 
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 2)}}

Revision as of 15:32, 4 February 2021

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching ICP Etching Oxygen Plasma Systems Other Dry Etchers
Material RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm) ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean) UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Ag A
Al A R R A
Au R
Cr A R A A
Cu A
Ge A A
Mo A
Ni R
Pt R
Ru A R A
Si R R R A
Ta A
Ti R A A
Al2O3 R A
Al2O3 (Sapphire) R A A
AlGaAs R R R A
AlGaN R A
AlN R A
CdZnTe R A
GaAs R R R R A
GaN R R R A
GaSb A R A
HfO2 A
InGaAlAs R R A
InGaAsP R R A
InP R A A R R
ITO R A
Photoresist

& ARC

A R R R A A A A
SiC R A A
SiN R R R A A
SiO2 R R R R R A
SiOxNy A A A
Ta2O5 A A
TiN A
TiO2 A
W-TiW R A A
ZnO2 A
ZnS R A
ZnSe R A
ZrO2 A
Material RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm) ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean) UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)