Difference between revisions of "Digital Microscope (Olympus DSX1000)"
(initial updates) |
|||
(3 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
− | {{ |
+ | {{tool2|{{PAGENAME}} |
|picture=OlympusDSX1000.jpg |
|picture=OlympusDSX1000.jpg |
||
|type = Inspection, Test and Characterization |
|type = Inspection, Test and Characterization |
||
|super= Tony Bosch |
|super= Tony Bosch |
||
+ | |super2= Demis D. John |
||
|location=Bay 4 |
|location=Bay 4 |
||
|description = Digital Optical Microscope |
|description = Digital Optical Microscope |
||
− | |manufacturer = [ |
+ | |manufacturer = [https://www.olympus-ims.com/en/microscope/dsx/ Olympus] |
|materials = |
|materials = |
||
}} |
}} |
||
− | = |
+ | =About= |
+ | The Olympus DSX1000 is a high-resolution digital microscope with full electronic control, multiple imaging modes and sophisticated analysis software built-in. |
||
− | The Olympus DSX1000... |
||
+ | The built-in optical magnification allows for high-resolution imaging without changing objectives. The system has applies Digital image stabilization and software image enhancement. |
||
⚫ | |||
⚫ | |||
⚫ | |||
− | Imaging Modes: Bright, Dark Field, DIC (Nomarski), |
||
⚫ | |||
⚫ | |||
+ | Users must be <u>very careful</u> to '''avoid crashing the 50x objective''', because it does not rotate out of the way like our other microscopes. |
||
⚫ | |||
+ | |||
⚫ | |||
⚫ | |||
+ | |||
+ | Optical Magnification ?? |
||
+ | |||
⚫ | |||
+ | |||
+ | Imaging Modes: Bright Field, Dark Field, DIC (Nomarski), Oblique Illumination (varying angle), Polarized Illumination (varying Pol.) |
||
+ | |||
⚫ | |||
+ | |||
⚫ | |||
+ | |||
⚫ | |||
[[Olympus DSX1000 - Quick Start|Olympus DSX1000 Quick Start.pdf]] |
[[Olympus DSX1000 - Quick Start|Olympus DSX1000 Quick Start.pdf]] |
||
− | === |
+ | ===Offline software=== |
− | [ |
+ | [[Olympus Stream Desktop Offline Software (TEMP)]] |
+ | |||
+ | == Other Info == |
||
+ | '''''Equip > Characterization > <u>[[Microscopes]]</u>''''' - ''see a list of all our microscopes'' |
Latest revision as of 11:49, 30 August 2022
|
About
The Olympus DSX1000 is a high-resolution digital microscope with full electronic control, multiple imaging modes and sophisticated analysis software built-in.
The built-in optical magnification allows for high-resolution imaging without changing objectives. The system has applies Digital image stabilization and software image enhancement.
Users must be very careful to avoid crashing the 50x objective, because it does not rotate out of the way like our other microscopes.
Technique & Capabilities
Digital only (view through computer)
Optical Magnification ??
Objectives: 5x, 50x
Imaging Modes: Bright Field, Dark Field, DIC (Nomarski), Oblique Illumination (varying angle), Polarized Illumination (varying Pol.)
Top Reflected Illumination (Episcopic)
Camera Capture: ??? MP
Operating Procedures
Olympus DSX1000 Quick Start.pdf
Offline software
Olympus Stream Desktop Offline Software (TEMP)
Other Info
Equip > Characterization > Microscopes - see a list of all our microscopes