Difference between revisions of "Dicing Saw (ADT)"
Jump to navigation
Jump to search
(Text replacement - "www.nanotech.ucsb.edu/wiki/" to "wiki.nanotech.ucsb.edu/wiki/") |
m |
||
(2 intermediate revisions by 2 users not shown) | |||
Line 27: | Line 27: | ||
== Recipes == |
== Recipes == |
||
− | * |
+ | * Recipes > Packaging > [https://wiki.nanotech.ucsb.edu/wiki/index.php/Packaging_Recipes?venotify=created#Dicing_Saw_Recipes_.28ADT_7100.29 '''Dicing Saw Recipes (ADT 7100)'''] |
− | Be sure to also see the |
+ | Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting. |
Revision as of 09:01, 23 September 2020
|
About
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the Dicing Saw Recipes page for the blades we currently stock.
An ADT WM-966 tape applicator & Ultron Systems UH104-8 UV lamp system is used to apply UV-release tape for securing die during dicing.
Contact the tool supervisor for blades and dicing frames for your group.
Detailed Specifications
Operating Procedures
- Setting up the Saw before Cutting
- Standard Dicing Procedure - Programmed Cut Map
- Standard Dicing Procedure - Single Cuts
- Recovering an Old Recipe
Recipes
- Recipes > Packaging > Dicing Saw Recipes (ADT 7100)
Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting.