Deep UV Optical Microscope (Olympus)
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
|
About
This system does general purpose imaging in the visible and also has high resolution/high magnification DUV imaging using 250 nm light. Surface features less than 100nm can be resolved.
The system has precision motorized stage control and is fully computer controlled for image capture and sample manipulation.
A Good system for CD measurements on wafer (250nm and above) without entry into the SEM.