Difference between revisions of "Chemical-Mechanical Polisher (Logitech)"
Jump to navigation
Jump to search
Freeborn d (talk | contribs) (CMP SOP) |
Freeborn d (talk | contribs) |
||
Line 18: | Line 18: | ||
Each process is often unique in geometry and material combinations so that independent process development is required for most CMP applications. |
Each process is often unique in geometry and material combinations so that independent process development is required for most CMP applications. |
||
− | =Instructions= |
+ | =[[Instructions]]= |
CMP SOP |
CMP SOP |
Revision as of 13:15, 23 August 2022
|
About
The Logitech Orbis system is used in the facility for fine-scale polishing and planarization of a variety of materials including glass, silicon, GaAs, InP, GaN, etc. Wafers up to 6” diameter can be polished on the system.
Several slurries and pads are available to provide a range of polishing options depending on the material being processed. Pieces can also be handled on the system by wax-mounting with the Logitech Bonder.
Each process is often unique in geometry and material combinations so that independent process development is required for most CMP applications.
Instructions
CMP SOP