Difference between revisions of "Automated Coat/Develop System (S-Cubed Flexi)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
m (fixed ToolTemplate 'type' arg)
(added ToolID (link to SUM))
Line 8: Line 8:
 
|type = Wet Processing
 
|type = Wet Processing
 
|recipe = Lithography
 
|recipe = Lithography
|materials =  
+
|materials =
|toolid=
+
|toolid=67
 
}}
 
}}
 
  '''THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.'''
 
  '''THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.'''

Revision as of 12:29, 13 November 2019

Automated Coat/Develop System (S-Cubed Flexi)
TBD.jpg
Tool Type Wet Processing
Location Bay 7
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Automatic Coat/Bake/Develop
Manufacturer S-Cubed
Model Flexi (Custom)
Wet Processing Recipes
Sign up for this tool


THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.

About

To Be Added

Detailed Specifications

  • Wafer Size: 100mm (150mm possible but not set up)
  • PR Coating Properties:
    • Uniformity < 1.0%
    • < 100 particles on 100mm wafer
  • Photoresists/Underlayers Available:
    • UV6-0.8
    • DS-K101-304
    • PMMA
    • PMGI SF11
    • PMGI SF5
  • Solvents Available:
    • EBR100
  • Developers Available:
    • AZ 300 MiF