Atomic Layer Deposition (Oxford FlexAL)

Al2O3 deposition (ALD)

AlN deposition (ALD)

HfO2 deposition (ALD)

SiO2 deposition (ALD)

ZrO2 deposition (ALD)

TiO2 deposition (ALD)

TiO2 recipe WJM_TDMAT_H2O_r2 water dose 1s, at 200C, gives grow rate 0.11 nm/cy (pdf file to be added)