The Oxford Instruments FlexAL Atomic Layer Deposition system at UCSB is a plasma-enhanced ALD system for the precise growth of ultra-thin oxides and nitrides. Self-limiting layer by layer growth ensures precise control, film conformality, and repeatability of the films. The system currently has metallorganic precursors for Aluminum, Hafnium, Zirconium, and Silicon oxides and nitrides. Water is available for thermal oxides and Oxygen, Nitrogen, and Hydrogen are available for plasma assisted oxides and nitrides. Remote ICP plasma powers up to 600W are possible. The system is load-locked and can accommodate sample temperatures up to 550°C. Processing temperature windows are defined for each material based on growth limitations. The system is step-by-step programmable through a flexible GUI interface. In-situ ellipsometry between growth cycles and mass spectrometry during growth are both available.
+
The Oxford Instruments FlexAL Atomic Layer Deposition system at UCSB is a plasma-enhanced ALD system for the precise growth of ultra-thin oxides and nitrides. Self-limiting layer by layer growth ensures precise control, film conformality, and repeatability of the films. The system currently has metallorganic precursors for Aluminum, Hafnium, Titanium, Platinum, Zirconium, and Silicon oxides and nitrides. Water and Ozone are available for thermal oxides and Oxygen, Ammonia, Nitrogen, and Hydrogen are available for plasma assisted oxides and nitrides. Remote ICP plasma powers up to 600W are possible. The system is load-locked and can accommodate sample temperatures up to 550°C. Processing temperature windows are defined for each material based on growth limitations. The system is step-by-step programmable through a flexible GUI interface. In-situ ellipsometry between growth cycles and mass spectrometry during growth are both available.
   
 
=Documentation=
 
=Documentation=

Revision as of 15:48, 13 July 2015

Atomic Layer Deposition (Oxford FlexAL)
FlexAL.jpg
Tool Type Vacuum Deposition
Location Bay 2
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description Oxford FlexAL Atomic Layer Deposition
Manufacturer Oxford Instruments Plasma Technologies
Vacuum Deposition Recipes
Sign up for this tool


About

The Oxford Instruments FlexAL Atomic Layer Deposition system at UCSB is a plasma-enhanced ALD system for the precise growth of ultra-thin oxides and nitrides. Self-limiting layer by layer growth ensures precise control, film conformality, and repeatability of the films. The system currently has metallorganic precursors for Aluminum, Hafnium, Titanium, Platinum, Zirconium, and Silicon oxides and nitrides. Water and Ozone are available for thermal oxides and Oxygen, Ammonia, Nitrogen, and Hydrogen are available for plasma assisted oxides and nitrides. Remote ICP plasma powers up to 600W are possible. The system is load-locked and can accommodate sample temperatures up to 550°C. Processing temperature windows are defined for each material based on growth limitations. The system is step-by-step programmable through a flexible GUI interface. In-situ ellipsometry between growth cycles and mass spectrometry during growth are both available.

Documentation

Etch Rates of ALD Films