Difference between revisions of "ASML 5500: Recovering from an Error"
Jump to navigation
Jump to search
(added instruciton to hit Help button) |
(Remove reticle) |
||
(2 intermediate revisions by the same user not shown) | |||
Line 1: | Line 1: | ||
− | # Do NOT exit |
+ | # '''Do NOT exit ''Task Streaming''!''' |
## If you exit the Task Streaming screen, the batch will not be able to be aborted, usually requiring a software reboot. |
## If you exit the Task Streaming screen, the batch will not be able to be aborted, usually requiring a software reboot. |
||
# If an "'''Abort Batch'''" Popup window appears: |
# If an "'''Abort Batch'''" Popup window appears: |
||
## Click the "'''Help'''" button, and take photos of the error chain |
## Click the "'''Help'''" button, and take photos of the error chain |
||
− | ## Click the "'''Help'''" button again, and write down timestamp of error in logbook/take screenshot - this helps engineer analyze the log file. |
+ | ## Click the "'''Help'''" button again, and write down timestamp of error in logbook/take screenshot - this helps an engineer analyze the log file. |
## Choose "'''Abort Batch, Clear Litho Cluster'''" - |
## Choose "'''Abort Batch, Clear Litho Cluster'''" - |
||
### This will send all your wafers through the stepper, from Port 1 → Port 2. Thus no wafers will be waiting for exposure. This is the easiest way to make sure all wafers are taken out of the machine. |
### This will send all your wafers through the stepper, from Port 1 → Port 2. Thus no wafers will be waiting for exposure. This is the easiest way to make sure all wafers are taken out of the machine. |
||
− | ## Wait for the task status to change from "Aborting" to " |
+ | ## Wait for the task status to change from "Aborting" to "Abort'''ed'''" |
# Abort the Batch: Make sure all batches say "Aborted" or "Completed". If not, choose the task from the Task List, click Batch > "Abort". May need to also click '''''Queue: Stop'''''. |
# Abort the Batch: Make sure all batches say "Aborted" or "Completed". If not, choose the task from the Task List, click Batch > "Abort". May need to also click '''''Queue: Stop'''''. |
||
+ | # Make sure the reticle was unloaded: (MAT HDL) > Remove Reticles From Machine |
||
− | Your wafer(s) should be removed to Port #2, and the task should state "Aborted" on the task list. |
+ | Your wafer(s) should be removed to Port #2, and the task should state "Aborted" on the task list. Only then is it safe to exit the ''Task Streaming'' screen. |
− | Please make sure there are no tasks in the "Waiting" state - please abort these tasks before leaving the system, or the next user's wafers will be shot with your job! |
+ | Please make sure there are no tasks in the "''Waiting''" state - please abort/cancel these tasks before leaving the system, or the next user's wafers will be shot with your job! |
Revision as of 14:46, 17 March 2020
- Do NOT exit Task Streaming!
- If you exit the Task Streaming screen, the batch will not be able to be aborted, usually requiring a software reboot.
- If an "Abort Batch" Popup window appears:
- Click the "Help" button, and take photos of the error chain
- Click the "Help" button again, and write down timestamp of error in logbook/take screenshot - this helps an engineer analyze the log file.
- Choose "Abort Batch, Clear Litho Cluster" -
- This will send all your wafers through the stepper, from Port 1 → Port 2. Thus no wafers will be waiting for exposure. This is the easiest way to make sure all wafers are taken out of the machine.
- Wait for the task status to change from "Aborting" to "Aborted"
- Abort the Batch: Make sure all batches say "Aborted" or "Completed". If not, choose the task from the Task List, click Batch > "Abort". May need to also click Queue: Stop.
- Make sure the reticle was unloaded: (MAT HDL) > Remove Reticles From Machine
Your wafer(s) should be removed to Port #2, and the task should state "Aborted" on the task list. Only then is it safe to exit the Task Streaming screen.
Please make sure there are no tasks in the "Waiting" state - please abort/cancel these tasks before leaving the system, or the next user's wafers will be shot with your job!