  1. Image.pngClick on the Programming Workspace
  2. Go to any recipe
  3. Click 'Recipe Import'Recipe import.png
  4. Select 'd: [New Volume]' from 'Folder List'

.......Volume d.jpg

  1. Open folder 'ADT'. Open Folder 'ADT-7100-8544150816'. Open folder 'db'. Open folder 'exports'
  2. Find you recipe in the box to the right and double click on it
  3. Verify group name is correct under 'Recipe Info'
  4. Click 'OK'
  5. Click 'Replace'
  6. Repeat for additional recipes